The part won't stick to the bed
The first layer comes loose, curls up, or the print ends as a tangle of spaghetti.
- Clean the bed: finger grease is the most common cause. Dish soap and warm water, or isopropyl alcohol.
- Check the nozzle height: the first layer should be slightly flattened (Z offset, bed leveling).
- Bed temperature as the filament asks for, around 60 °C for PLA.
- Add a brim for small contact areas: an extra rim that holds the part down.
Corners lift (warping)
The corners bend upwards and the part ends up crooked. Plastic shrinks as it cools, and large flat parts pull up at the corners.
- Use a brim and keep the bed clean.
- Avoid drafts: no open window or air conditioner next to the printer.
- For PETG, ASA and ABS: a warmer bed, and for ASA and ABS an enclosed printer.
Fine strings between parts (stringing)
Thin strings hang between two spots like cobwebs. Melted filament oozes out of the nozzle while it travels.
- Turn on retraction or increase it a little.
- Lower the temperature by 5 to 10 °C.
- Dry the filament: damp filament strings much more, especially PETG and TPU.
Small strings can simply be pulled or cut off after printing.
The bottom edge sticks out (elephant's foot)
The bottom layer is wider than the rest, and the part doesn't fit at the bottom. The first layer was pressed too hard onto the hot bed.
- Raise the nozzle slightly for the first layer.
- Lower the bed temperature a little.
- Use elephant's foot compensation in the slicer if it has one.
Overhangs sag
Sloped or flat parts get wavy underneath or droop. The plastic has nothing to rest on in mid-air.
- Fan at full speed (for PLA).
- Place the part differently on the bed so less of it hangs in the air.
- Up to about 45° almost always works without supports; anything flatter needs supports or a different orientation.
- Short bridges, straight runs between two supports, up to about 20 mm work on almost any printer.
Gaps and thin walls (under-extrusion)
The walls have gaps, the surface is full of holes or the part is brittle. Too little filament comes out of the nozzle.
- Check that the spool turns freely and the filament isn't tangled.
- Partly clogged nozzle? Clean it, for example with a cold pull, or replace it.
- Print more slowly or raise the temperature a little.
- Dry the filament.
Layers shifted (layer shift)
From a certain height the whole part is offset to one side. The print head lost steps, for example because it hit the part or a belt is loose.
- Check the belts: they should be taut.
- Print more slowly.
- Avoid lifted corners (see warping) that the nozzle can catch on.
Moving parts are stuck together
A print-in-place part won't move. Usually the first layer is too flat or the gap is too narrow for your printer. All about it in Printing moving parts in one piece.
Tools for this